标题 |
Fig. 11. Conversion of furfural and the selectivity of the formation of its hydrogenation products depending on the reaction time on Ru catalysts deposited on: (a) mesoporous nanospheric polymer; (b) Mesoporous zircon silicate; (c) mesoporous material based on carbon nanospheres and zirconosilicate. * Reaction conditions: 170 °C, 3 MPa H2, 50 µl of furfural, 4 mg of catalyst, 2 ml of water. ** Others: 2-methylfuran, tetrahydro-2-methylfuran, tetrahydrofurfural, pentanol, pentanediol-1,4, 3-acetyl-1- propanol, 2-cyclopentenone, 4-gyroxy-2-cyclopentenone, 2- furfuryl-5-methylfuran, difurfuryl ether. |